Hobbing cuts the flank.
The tester checks it.
The flank of a gear is made in one pass of a hob, and that pass decides how much the furnace and the grinder can still correct. We cut external spur and helical teeth on our own hobbing machines, shape the internal teeth and herringbones a hob cannot reach, and measure the gear on the tester before it leaves.
Tolerances, heat treatment and inspection
These are the working limits on a normal order. They are confirmed against the drawing and the material before the first cut.
Tolerances and accuracy
- Size-dependent tolerance: ±0.02 mm (0–500 mm), ±0.05 mm (500–2,000 mm), ±0.1 mm above 2,000 mm; ISO IT grades on request.
- Coaxiality 0.02–0.05 mm; face runout ≤0.03 mm; roundness and parallelism are recorded at inspection.
- Turning Ra 3.2–6.3 µm; grinding Ra 0.8–1.6 µm.
- Gear accuracy to ISO 1328 / DIN 3962: hobbing grade 8, profile grinding grades 4–7 as specified.
Heat treatment
- Quenching and tempering: HB 220–320.
- Hardening: HRC 40–58.
- Carburizing: surface HRC 58–62, effective case 0.8–4 mm.
- Nitriding: surface HV 800–1,100, case 0.1–0.6 mm.
- Run to the drawing and ISO/AGMA/ASTM standards, with hardness reports.
Inspection and third-party testing
- UT, MT and PT in-house by certified personnel; RT subcontracted to an accredited laboratory.
- Reports to ASME and GB standards; customer or third-party witness is welcome.
- SGS, BV, TÜV or Intertek can inspect at our works; the buyer bears the cost by default, negotiable on large orders.
- Material certificates and dimensional records are traceable and can travel with the shipment.
Lead time
- Small single parts: 2–4 weeks.
- Small batches: 3–6 weeks.
- Large parts: 8–12 weeks.
- The date is confirmed after drawing review; size, module, heat treatment and inspection scope can extend it.
The route a gear takes here
Six operations, in this order. Stress is relieved before the teeth are cut and the gear is measured again after hardening — the order is what keeps the flank where the drawing put it.
Blank and certificate
A casting, forging or rolled ring with its mill certificate. Stress relieved before turning, or the teeth move later.
Rough turning, quench and temper
Brought to size with allowance, structure evened out, so the blank behaves under the cutter.
Finish turning
Mounting face, bore and the datum the teeth are referenced to.
Hobbing or shaping
External spur and helical teeth on the hob; internal teeth, herringbones and shoulders on the shaper.
Hardening
Induction hardening of the tooth surface. The gear is measured again to see what the heat moved.
Grinding and inspection
Ground flanks where the drawing calls for them; profile, lead, pitch and runout recorded on the tester.
What the cut decides
The hob generates the whole flank in one pass: profile, helix and pitch are set by the machine, the cutter and the blank, in that order. A gear that leaves hobbing out of profile cannot be ground into shape economically — grinding removes material, it does not put it back. That is why the module and the accuracy grade are agreed at drawing review, before a cutter is chosen.
Hobbing, shaping, and the teeth a hob cannot reach
A hob is a screw-shaped cutter that rolls against the blank, and it cuts external spur and helical teeth faster than any other method. It cannot enter an internal tooth, a herringbone, or a flank beside a shoulder. Those go on the shaping machine, where a reciprocating cutter works one tooth space at a time. Both machines stand in the same workshop as the lathes that turn the blank.
The grade on the drawing is several measurements
An accuracy grade is not one number. Pitch deviation, total cumulative pitch error, profile form, helix deviation and runout are measured separately, and the grade applies to all of them. At drawing review we confirm which of them the drawing controls, because they decide the cutter, the number of passes and how the blank is set.
Heat treatment moves the teeth
Hardening is where a machined gear stops being predictable. The surface grows, the ring distorts, and a flank that measured true before the furnace is no longer true after it. The gear is measured before hardening and after; the difference is what grinding has to take off, and it has to be on the drawing as an allowance before the first cut.
What ships with the gear
A dimensional record, hardness readings, the material certificate, and whatever tooth measurements the drawing asks for. Export crates carry lifting points and rust protection, and inspection reports are issued in English.
Common questions
- What is the largest gear you can hob?
- Eight meters outside diameter as one piece, ten meters for a ring assembled from sections. Below that the limit is the module and the grade rather than the size.
- Can you cut internal teeth?
- Yes, on the shaping machine: internal teeth, herringbones, and gears with a shoulder the hob cannot pass.
- Do I need to send a drawing?
- A drawing is the fastest route. Without one, send the gear or its mating part; we measure module, tooth count and helix angle and issue a drawing for your approval.
- How long does a gear take?
- Usually eight to twelve weeks from the approved drawing, depending on diameter, module and heat treatment. The date is confirmed with the quotation.
- Which steel do you cut?
- The grade the drawing names, verified against the mill certificate on arrival. Where the grade has to be substituted, the alternative is agreed with you before the blank is turned.
Send the drawing, or the gear data.
Module, tooth count, outside diameter and accuracy grade are enough to quote. Without a drawing, we measure the sample first.
Send a drawing or a photo