Tests happen where
the part can fail.
A test is worth what it is done at. Ultrasonic testing means something on the blank, before a defect is buried under a finished surface; magnetic particle testing means something after hardening, when cracks have started. This page is about which test happens when, what it finds, and what the report actually says.
Tolerances, heat treatment and inspection
These are the working limits on a normal order. They are confirmed against the drawing and the material before the first cut.
Tolerances and accuracy
- Size-dependent tolerance: ±0.02 mm (0–500 mm), ±0.05 mm (500–2,000 mm), ±0.1 mm above 2,000 mm; ISO IT grades on request.
- Coaxiality 0.02–0.05 mm; face runout ≤0.03 mm; roundness and parallelism are recorded at inspection.
- Turning Ra 3.2–6.3 µm; grinding Ra 0.8–1.6 µm.
- Gear accuracy to ISO 1328 / DIN 3962: hobbing grade 8, profile grinding grades 4–7 as specified.
Heat treatment
- Quenching and tempering: HB 220–320.
- Hardening: HRC 40–58.
- Carburizing: surface HRC 58–62, effective case 0.8–4 mm.
- Nitriding: surface HV 800–1,100, case 0.1–0.6 mm.
- Run to the drawing and ISO/AGMA/ASTM standards, with hardness reports.
Inspection and third-party testing
- UT, MT and PT in-house by certified personnel; RT subcontracted to an accredited laboratory.
- Reports to ASME and GB standards; customer or third-party witness is welcome.
- SGS, BV, TÜV or Intertek can inspect at our works; the buyer bears the cost by default, negotiable on large orders.
- Material certificates and dimensional records are traceable and can travel with the shipment.
Lead time
- Small single parts: 2–4 weeks.
- Small batches: 3–6 weeks.
- Large parts: 8–12 weeks.
- The date is confirmed after drawing review; size, module, heat treatment and inspection scope can extend it.
The gates a part passes
Tests are placed on the route at the points where the evidence exists, and the record is built as the part is, not after it.
Incoming material
The grade is checked against the mill certificate before anything is cut. Ultrasonic testing is applied here, on the blank, where the drawing asks for it.
Rough and finish machining
Dimensions are held to the datums the drawing names, and in-process checks keep the finishing allowance where the route put it.
Hardening
Induction hardening of the tooth or journal surface, with the parameters set from the grade and the case depth the drawing requires.
Magnetic particle and hardness
After hardening, surfaces are checked for cracks and hardness is measured where the drawing says — surface, case depth, or a coupon from the same heat.
Final measurement
Bores, journals, tooth pitch, runout and whatever tolerance the drawing controls, recorded on the part that actually ships.
The report
Material certificate, test results and the dimensional record travel with the part, in English, or on your template if one comes with the enquiry.
What ultrasonic testing finds, and what it needs
Inside a casting or a forging: porosity, inclusions, shrinkage and forging bursts, before machining turns them into a scrapped part. UT needs a surface the probe can couple to and a standard to judge against. Coverage — a full scan or a defined path — and the acceptance level are drawing decisions; without them a report is a list of readings with nothing to measure them against.
Why magnetic particle testing comes after the furnace
Hardening and grinding are where surface cracks start. Magnetic particle testing finds surface and near-surface discontinuities in ferromagnetic steel quickly, over a whole flank or journal. It does not look inside the part — that is what UT is for — and it does not work on austenitic stainless or other non-magnetic material, which has to be tested another way.
What induction hardening is measured by
An induction coil heats the surface and the surface is quenched, so the tooth or the journal gets a hard case while the core stays tough. The result is judged by case depth, surface hardness and the transition between them, measured on a coupon from the same heat or by a hardness traverse where the drawing allows. Distortion is measured too: a hardened ring is not the ring that was cut.
The report, and the standard behind it
A report that means something names the material, the heat treatment, the method, the standard, the coverage and the results in the units the drawing uses. If a plant, a yard or a class society works to a template, send it with the enquiry and we confirm what we can issue before quoting. We do not claim an approval we have not been given.
What to put on the drawing
The method, the standard, the coverage, the acceptance level, and the position for hardness. Where the drawing is silent we ask before the test, not after: a test performed without an acceptance level can be neither passed nor failed, and a part held at the gate costs both sides time.
Common questions
- Do you do UT and MT in-house?
- Yes. Ultrasonic, magnetic particle, hardness, tensile and impact testing are done in our own laboratory, and reports can be issued in English for export orders.
- Can you test to our own standard?
- Send the standard and the acceptance level with the enquiry. We confirm that the method, the coverage and the report will match it before quoting, and say so at that point if something cannot be met.
- Do you inspect after hardening?
- Hardened surfaces are checked for cracks by magnetic particle testing, and hardness is measured where the drawing specifies. Case depth is verified on a coupon from the same heat, or by the method the drawing names.
- What happens if a test fails?
- The part does not ship. We report the result, the position and the size of the indication, and what the options are: rework, replacement, or a concession you agree to. The decision is yours, made on the evidence.
- How much time do the tests add?
- They run inside the route rather than after it: UT on the blank, hardness after hardening, final measurement before packing. The delivery date quoted already includes them.
Send the drawing and the test standard.
Method, coverage, acceptance level and the position for hardness are what a test needs. If they are not on the drawing yet, we list what to add before the first cut.
Send a drawing or a photo