The teeth move in heat.
Grinding sets them.
A hardened gear is not a finished gear. Quenching grows the surface and distorts the ring, so the flank that was true when it left the hob is no longer true. Grinding takes that movement out and puts the flank back where the drawing put it — an operation that belongs after the furnace, not instead of it.
Tolerances, heat treatment and inspection
These are the working limits on a normal order. They are confirmed against the drawing and the material before the first cut.
Tolerances and accuracy
- Size-dependent tolerance: ±0.02 mm (0–500 mm), ±0.05 mm (500–2,000 mm), ±0.1 mm above 2,000 mm; ISO IT grades on request.
- Coaxiality 0.02–0.05 mm; face runout ≤0.03 mm; roundness and parallelism are recorded at inspection.
- Turning Ra 3.2–6.3 µm; grinding Ra 0.8–1.6 µm.
- Gear accuracy to ISO 1328 / DIN 3962: hobbing grade 8, profile grinding grades 4–7 as specified.
Heat treatment
- Quenching and tempering: HB 220–320.
- Hardening: HRC 40–58.
- Carburizing: surface HRC 58–62, effective case 0.8–4 mm.
- Nitriding: surface HV 800–1,100, case 0.1–0.6 mm.
- Run to the drawing and ISO/AGMA/ASTM standards, with hardness reports.
Inspection and third-party testing
- UT, MT and PT in-house by certified personnel; RT subcontracted to an accredited laboratory.
- Reports to ASME and GB standards; customer or third-party witness is welcome.
- SGS, BV, TÜV or Intertek can inspect at our works; the buyer bears the cost by default, negotiable on large orders.
- Material certificates and dimensional records are traceable and can travel with the shipment.
Lead time
- Small single parts: 2–4 weeks.
- Small batches: 3–6 weeks.
- Large parts: 8–12 weeks.
- The date is confirmed after drawing review; size, module, heat treatment and inspection scope can extend it.
Where grinding sits in the route
Grinding is the last cut a gear receives, and it exists because of the operation before it.
Hobbing
The flank is generated in the soft state, with an allowance on tooth thickness for what comes next.
Hardening
Induction hardening of the tooth surface. The ring and the flank both move.
Measurement
The gear is checked against the drawing to see what the heat did.
Grinding
Profile and lead are corrected until the flank is back on the drawing.
Inspection
The finished flank is measured again, and the record ships with the gear.
Why a hardened gear is not a finished gear
Quenching leaves the tooth surface harder and the whole ring less true. Distortion is not uniform: the ring can go oval, the flank can lean, and the pitch can shift along the face. A hard surface does not take a cutter, so once the gear has been quenched the flank can only be corrected by grinding.
What grinding corrects, and what it cannot
Grinding corrects profile form, lead deviation, pitch and surface finish, within the allowance left on the tooth. It does not add case depth. A flank ground past the hardened layer is soft again, and a tooth ground too deep is thin — which is why the allowance is a drawing decision made together with the heat treatment, not something settled at the machine.
Three numbers that have to agree
Tooth thickness, case depth and grinding allowance are one decision, not three. An allowance too small leaves distortion that cannot be removed; an allowance too large eats the case and takes tooth thickness the gear needs for backlash. Both are settled before the blank is turned.
What we need to quote a ground gear
Outside diameter, module, face width, tooth count, helix angle, the accuracy grade the drawing calls for, and the heat treatment the gear will receive. With those, the machine and the number of passes are confirmed before a price is given.
Measured on the finished flank
The record that matters is taken after grinding: profile, lead, pitch and runout on the gear tester, plus surface roughness where the drawing names it. Measurements taken before the furnace describe a different gear.
Common questions
- Do you grind the teeth after hardening?
- Yes. Tooth flanks are ground after heat treatment on our own machine, and the finished flank is measured before the gear is packed.
- How large a gear can you grind?
- Send the outside diameter, module and face width and we confirm against the machine before quoting. The diameter sets the limit first, then the module.
- Does grinding change the backlash?
- Grinding thins the tooth by the allowance, so backlash grows unless the drawing accounts for it. If you are matching an existing gear, state the backlash you need and the allowance is set to hit it.
- Can a worn gear be reground?
- Only where tooth thickness above the hardened case is left. Once the case is worn through, the part is a replacement rather than a regrind, and we say which before quoting.
- How long does it take?
- Grinding runs inside the gear route: a ground gear usually takes eight to twelve weeks from the approved drawing, hardening and grinding included.
Send the gear data, or the drawing.
Diameter, module, face width, grade and heat treatment are enough to confirm the machine and the allowance.
Send a drawing or a photo