Two grades, two jobs.
The section decides.
42CrMo4 and 34CrNiMo6 are the two grades most drawings name for large shafts, gears and rings. This page is about what each one is chosen for — and why the numbers printed in a steel catalog do not travel to the core of a 600 mm section.
Tolerances, heat treatment and inspection
These are the working limits on a normal order. They are confirmed against the drawing and the material before the first cut.
Tolerances and accuracy
- Size-dependent tolerance: ±0.02 mm (0–500 mm), ±0.05 mm (500–2,000 mm), ±0.1 mm above 2,000 mm; ISO IT grades on request.
- Coaxiality 0.02–0.05 mm; face runout ≤0.03 mm; roundness and parallelism are recorded at inspection.
- Turning Ra 3.2–6.3 µm; grinding Ra 0.8–1.6 µm.
- Gear accuracy to ISO 1328 / DIN 3962: hobbing grade 8, profile grinding grades 4–7 as specified.
Heat treatment
- Quenching and tempering: HB 220–320.
- Hardening: HRC 40–58.
- Carburizing: surface HRC 58–62, effective case 0.8–4 mm.
- Nitriding: surface HV 800–1,100, case 0.1–0.6 mm.
- Run to the drawing and ISO/AGMA/ASTM standards, with hardness reports.
Inspection and third-party testing
- UT, MT and PT in-house by certified personnel; RT subcontracted to an accredited laboratory.
- Reports to ASME and GB standards; customer or third-party witness is welcome.
- SGS, BV, TÜV or Intertek can inspect at our works; the buyer bears the cost by default, negotiable on large orders.
- Material certificates and dimensional records are traceable and can travel with the shipment.
Lead time
- Small single parts: 2–4 weeks.
- Small batches: 3–6 weeks.
- Large parts: 8–12 weeks.
- The date is confirmed after drawing review; size, module, heat treatment and inspection scope can extend it.
The same questions, two answers
42CrMo4
1.7225 · AISI 4140 · GB 42CrMo · EN 10083-3
Chromium-molybdenum steel with about 0.4 % carbon. It quenches and tempers predictably, machines well, and carries most of the gears, shafts, flanges and rings we cut. Chosen when the section is moderate and the duty is heavy but not punishing.
34CrNiMo6
1.6582 · EN 10083-3
Nickel added for toughness and hardenability. It holds a sound core in sections where 42CrMo4 has already begun to lag, which is why wind turbine main shafts and highly stressed journals are drawn in it. Chosen when the part is large, the load reverses, or the core has to carry properties as well as the surface.
What a grade name actually promises
A grade fixes the chemistry and the standard it is made to. The figures in a steel data sheet — yield, tensile, impact — are measured on small test pieces, quenched and tempered on their own and tested at a stated position. A 600 mm section cools more slowly than a 25 mm bar, so its core does not reach the same structure or the same numbers. The grade is a starting point; the section, the heat treatment and the test position decide the rest.
42CrMo4 in the parts we cut
Gear blanks, pinions, shafts, flanges and rolled rings. It takes a good finish, induction-hardens cleanly on tooth and journal surfaces, and stays stable through the second heat treatment. For most of the machinery parts that arrive here it is the grade the drawing names, and it is usually the right one.
When nickel earns its price
34CrNiMo6 costs more and machines harder, so it is specified for a reason: a large section that must stay tough to the core, a reversing load, a journal that cannot be allowed to fail. Large parts in this grade usually arrive as forgings, with the forging ratio and the ultrasonic test agreed at drawing review. It is not a drop-in upgrade for 42CrMo4 — welding, machining and distortion all change with it.
Heat treatment is a route, not one step
Stress relief before rough machining, quench and temper before the teeth are cut, induction hardening after, then tempering again. Every step moves the part, and the allowance for each is set at drawing review. Hardness is measured where the drawing says — surface, case depth, or a coupon cut from the same heat — because a reading taken anywhere else describes a different part.
The steel we buy, and what ships with it
Blanks come as castings, forgings or rolled rings with their mill certificate, and the grade is checked on receipt before anything is cut. Ultrasonic testing is applied where the drawing asks for it. Any substitution is proposed in writing and waits for your agreement. The certificate, the dimensional record and the hardness results travel with the part, in English.
Common questions
- Can 34CrNiMo6 replace 42CrMo4?
- Only with your engineering agreement. It is tougher and more hardenable, but it welds and machines differently and costs more. We propose the substitution and wait; we do not make it quietly.
- Which certificate do we receive?
- The mill certificate that came with the steel, plus our hardness and dimensional records. If your drawing names a certificate type or a third-party inspection, send it with the enquiry so we can confirm before quoting.
- Do you ultrasonic test the forging?
- Where the drawing asks for it. The standard, the coverage and the acceptance level have to be on the drawing or agreed before the test, so tell us which one applies to the part.
- What do you need to quote a blank?
- Grade and standard, the drawing with its heat treatment and hardness, the section or the finished weight, and the test requirements. With those, the blank, the route and the date can be quoted together.
- How long does a part in these grades take?
- Usually eight to twelve weeks from the approved drawing, heat treatment included. If the grade or the section has to be forged to order, the material lead time is added and stated in the quotation.
Send the drawing and the grade.
Grade, standard, heat treatment and section are enough to quote the blank and the machining. If the grade is still open, we propose one and say why.
Send a drawing or a photo